40/50 liter resin with phosphating agent
Specially designed for use in old rusty or micro-perforated tanks. Also recommended for it
sealing tanks from your own production to prevent leaks at different welds.
The operation is easy if all methods are well respected, because we know what we do not know from experience
must do. Just like when cooking, certain rules and temperatures must be observed to it
obtain the best result. The resin must be used at a temperature above 20 ° to control the catalyst
ignite. Resin must be used if there is no moisture, therefore in very dry tanks. When in doubt
a switch to acetone is recommended. Acetone is an excellent drying product. Always pay attention to the threads
and fillings to be clogged during rust removal and during resin. And especially in the curing phase
of the resin just before ventilation, so that the threads are not absorbed by the resin (take them again with one
some acetone). Perhaps the most important thing is ventilation after the resin has hardened if it is frozen but still
is not dry. We have tried everything, be sure and the best is the enemy of the good, so try ours
do not replace national hair dryer with a stripper or fan or blow gun or what we do not know exist
but the last in cold position or the least warm at 10 cm or by going backwards a bit like the warm the
smallest position. And then not 5 minutes or 10 minutes or 30 minutes, but until the resin has to be marbled
and not sticky on the finger as if you are touching glass. We have tried everything we believe and it is the best recipe
this. Depending on the temperature and humidity it can take 3/4 to 2 hours. Here we do not have the exact
science but the certainty of the result. After this operation you must have your minimum tank 8 to 10 days on one
leave a ventilated place before refueling. Be soothed by our knowledge and not by our pride and ours
publicity brings yes.